XLPE Polylink Power Cable PP 409/401 (S) Polylink Polymers (India) Ltd.

0
  • Properties:
    Thermal performance

Technical Data Sheet

Test ConditionTest MethodTest Result
thermosettingIEC 608115.0 %
Volume resistivityIEC 605021.4E+17 ohms·cm
dielectric strengthIEC 60243-125 kV/mm
dielectric constantIEC 602502.20
Loss factorIEC 2504E-04
densityASTM D15050.925 g/cm³
melt mass-flow rateASTM D12380.75 g/10min
tensile strength BreakIEC 6081114.5 MPa
Tensile strainBreakIEC 60811400 %
Change rate of tensile strength in airIEC 6081115 %
Tensile stress change rateIEC 6081110 %
thermosettingIEC 60811100 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.