PP+EPDM TPV Elastoprene® N60A-i Elastómeros Riojanos S.A.

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO 1183/A0.960 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardnessISO 86860
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94HB
Supplementary InformationTest ConditionTest MethodTest Result
ozone resistanceISO 1431-10Rating
elastomerTest ConditionTest MethodTest Result
tensile strength ISO 371.70 MPa
tensile strength ISO 374.00 MPa
elongationISO 37320 %
tear strengthISO 34-16.0 kN/m
compression setISO 81533 %
Thermal performanceTest ConditionTest MethodTest Result
brittle temperatureISO 812-62.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.