Test Condition | Test Method | Test Result | |
---|---|---|---|
热变形温度 | 1.8MPa,未退火 | ASTMD648 | 87.8 °C |
UL阻燃等级 | 1.5mm | 内部方法 | V-0 |
3.0mm | 内部方法 | 5VA | |
密度 | ASTMD792 | 1.20 g/cm³ | |
熔体质量流动速率 | 220°C/10.0kg | ASTMD1238 | 11 g/10min |
260°C/5.0kg | ASTMD1238 | 38 g/10min | |
收缩率 | MD | ASTMD955 | 0.60到0.90 % |
抗张强度 | Yield | ASTMD638 | 54.5 MPa |
伸长率 | Break | ASTMD638 | 90 % |
弯曲模量 | ASTMD790 | 2390 MPa | |
弯曲强度 | ASTMD790 | 82.7 MPa | |
悬壁梁缺口冲击强度 | 23°C | ASTMD256 | 590 J/m |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.