| optical performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| gloss | 45°,20.3um | ASTM D-2457 | 95 | |
| turbidity | 20.3um | ASTM D-1003 | 0.4 | % |
| gloss | 45°,20.3μm | ASTM D2457 | 95 | |
| turbidity | 20.3μm | ASTM D1003 | 0.40 | % |
| Other performance | Test Condition | Test Method | Test Result | Test Unit |
| Thin film puncture strength | 20.3um | Internal Method | 22.1 | J/cm³ |
| Film toughness | 20.3um,TD | ASTM D-882 | 171 | J/cm³ |
| 20.3um,MD | ASTM D-882 | 176 | J/cm4 | |
| Basic Performance | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D-792 | 0.917 | g/m3 | |
| melt mass-flow rate | 190℃/2.16kg | ASTM D-1238 | 2.3 | g/10min |
| film thickness | 20.3 | um | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | 20.3um,Yield,MD | ASTM D-882 | 8.79 | Mpa |
| 20.3um,Yield,TD | ASTM D-882 | 8.16 | Mpa | |
| 20.3um,MD,Break | ASTM D-882 | 20.1 | Mpa | |
| 20.3um,TD,Break | ASTM D-882 | 28.8 | Mpa | |
| Elongation at Break | 20.3um,MD | ASTM D-882 | 460 | % |
| 20.3um,TD | ASTM D-882 | 650 | % | |
| Dart impact | 20.3um | ASTM D-1709B | 210 | g |
| Elmendorf tear strength | 20.3um,TD | ASTM D-1922 | 510 | g |
| 20.3um,MD | ASTM D-1922 | 340 | g | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | ASTM D-1525 | 97.8 | °C | |
| Melting temperature | Internal Method | 122 | °C | |
| Vicat softening temperature | ASTM D1525 | 97.8 | °C | |
| Melting temperature | Internal Method | 122 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D792 | 0.917 | g/cm³ | |
| melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 2.3 | g/10min |
| film | Test Condition | Test Method | Test Result | Test Unit |
| film thickness | 20 | µm | ||
| Thin film puncture strength | 20μm | Internal Method | 22.1 | J/cm³ |
| Membrane strength | MD:20μm | ASTM D882 | 176 | J/cm³ |
| TD:20μm | ASTM D882 | 171 | J/cm³ | |
| tensile strength | MD:Yield,20μm | ASTM D882 | 8.79 | Mpa |
| TD:Yield,20μm | ASTM D882 | 8.16 | Mpa | |
| MD:Break,20μm | ASTM D882 | 50.1 | Mpa | |
| TD:Break,20μm | ASTM D882 | 28.8 | Mpa | |
| elongation | MD:Break,20μm | ASTM D882 | 460 | % |
| TD:Break,20μm | ASTM D882 | 650 | % | |
| Dart impact | 20μm | ASTM D1709A | 210 | g |
| Elmendorf tear strength | MD:20μm | ASTM D1922 | 340 | g |
| TD:20μm | ASTM D1922 | 510 | g |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.