Share
Add to compare

PC LUX 2180T SABIC INNOVATIVE NANSHA

46

Form:Granules | Grade:Transparent level

Properties:
OpticsUV resistanceAging resistanceWeather resistanceHigh impact resistance
Typical Applications:
Lighting applications
Product Description
Certificates(0)
Datasheet

Product Description

Typical Applications:Lighting applications
Properties:Optics | UV resistance | Aging resistance | Weather resistance | High impact resistance

Certificates

No Data...

Technical Data Sheet

optical performanceTest ConditionTest MethodTest ResultTest Unit
Refractive indexISO 4891.586
Transmittance rate2540μmASTM D1003>90.0%
Transmittance rate2540μm,420nmInternal Method>88.0%
Transmittance rate5000μmInternal Method>89.0%
turbidity2540μmASTM D1003<0.50%
flammabilityTest ConditionTest MethodTest ResultTest Unit
UL flame retardant rating0.800mmUL 94V-2
Burning wire flammability index1.00mmIEC 60695-2-12850°C
Hot filament ignition temperature1.00mmIEC 60695-2-13>875°C
Extreme Oxygen IndexISO 4589-225%
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
Impact strength of simply supported beam without notch23°CISO 179/1eU无断裂
Impact strength of cantilever beam gap-30°CISO 180/1A15kJ/m²
Impact strength of cantilever beam gap23°CISO 180/1A65kJ/m²
Suspended wall beam without notch impact strength-30°CISO 180/1U无断裂
Suspended wall beam without notch impact strength23°CISO 180/1U无断裂
tensile strengthYieldISO 527-2/5062.0Mpa
tensile strengthBreakISO 527-2/5069.0Mpa
Tensile strainYieldISO 527-2/506.0%
Tensile strainBreakISO 527-2/50100%
Bending modulusISO 1782300Mpa
bending strengthISO 17890.0Mpa
Taber abraser1000Cycles,1000g,CS-17WheelInternal Method10.0mg
Charpy Notched Impact Strength-30°CISO 179/1eA12kJ/m²
Charpy Notched Impact Strength23°CISO 179/1eA65kJ/m²
Impact strength of simply supported beam without notch-30°CISO 179/1eU无断裂
Ball Pressure TestH358/30ISO 2039-195.0Mpa
Tensile modulusISO 527-2/12350Mpa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
0.45MPa, unannealed, 100mm spanISO 75-2/Be133°C
1.8MPa, unannealed, 100mm spanISO 75-2/Ae122°C
--ISO 306/B50140°C
--ISO 306/B120141°C
Ball Pressure Test125°CIEC 60695-10-2Pass
Linear coefficient of thermal expansionMD:23to80°CISO 11359-27E-05cm/cm/°C
thermal conductivityISO 83020.20W/m/K
RTI ElecUL 746130°C
RTI ImpUL 746125°C
RTIUL 746125°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
Melt Volume Flow Rate (MVR)300°C/1.2kgISO 113318.0cm3/10min
Shrinkage rateMD1Internal Method0.50-0.70%
Water absorption rateSaturation,23°CISO 620.35%
Water absorption rateEquilibrium,23°C,50%RHISO 620.15%
Outdoor applicabilityUL 746Cf1
Electrical performanceTest ConditionTest MethodTest ResultTest Unit
Relative permittivity1MHzIEC 602502.70
Dissipation factor50HzIEC 602501E-03
Dissipation factor60HzIEC 602501E-03
Dissipation factor1MHzIEC 602500.010
Surface resistivityIEC 60093>1.0E+15ohms
Volume resistivityIEC 60093>1.0E+15ohms·cm
Dielectric strength3.20mm,in OilIEC 60243-117KV/mm
Relative permittivity50HzIEC 602502.70
Relative permittivity60HzIEC 602502.70
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.