Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.87 g/cm³ |
Water absorption rate | Equilibrium | ASTMD229 | 0.60 % |
hardness | Test Condition | Test Method | Test Result |
---|
Barcol Hardness | | | 46 |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | HB |
FlameResistance | | ASTMD229 | 5.5 min |
FlameResistance | | ASTMD229 | 1.0 min |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
BondStrength | | ASTMD229 | 8.62 MPa |
Temperature Rating | | | 130 °C |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTMD638 | 68.9 MPa |
Flexural modulus | | ASTMD790 | 6890 MPa |
bending strength | | ASTMD790 | 159 MPa |
compressive strength | | ASTMD695 | 207 MPa |
shear strength | | ASTMD732 | 96.5 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 430 J/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|
dielectric constant | | ASTMD150 | 4.80 |
dielectric constant | | ASTMD150 | 4.30 |
Dissipation Factor | | ASTMD150 | 0.015 |
Dissipation Factor | | ASTMD150 | 0.011 |
arc resistance | | ASTMD495 | 150 sec |
Dielectric strength Step By Step InOil | | ASTMD149 | 54000 V |
dielectric strength | | ASTMD149 | 20 kV/mm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.