PS Resan SAN Polimarky Spolka Jawna
0
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1A | 2.0to10 kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Tensile modulus | ISO 527-2 | 2100to3100 MPa | |
| tensile strength | ISO 527-2 | 20.0to23.0 MPa | |
| Tensile strain | Break | ISO 527-2 | 2.0to30 % |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 73.0 °C |
| Vicat softening temperature | ISO 306/A120 | 91.0 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | ISO 1183 | 1.04to1.07 g/cm³ | |
| melt mass-flow rate | 200°C/5.0kg | 6.0to13 g/10min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.