PC 1260C 700394 COVESTRO SHANGHAI
112
Form:Granules | Grade:Wear resistant grade
Properties:
Impact modificationLow viscosityGood demolding performanc
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | Impact modification | Low viscosity | Good demolding performanc |
Certificates
No Data...
Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| tensile strength | 23°C | ISO 527-2 | 63.0 | Mpa |
| Elongation at Break | 23°C | ISO 527-2 | >50 | % |
| Tensile modulus | 23°C | ISO 527-2 | 2350 | Mpa |
| bending strength | 23°C | ISO 178 | 93.0 | Mpa |
| Bending modulus | 23°C | ISO 178 | 2350 | Mpa |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 55 | kJ/m² |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 65 | kJ/m² |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 7E-05 | cm/cm/°C |
| Hot deformation temperature | 0.45MPaUnannealed | ISO 75-2/Bf | 135 | °C |
| 1.80MPaAnnealed | ISO 75-2/Af | 122 | °C | |
| Vicat softening temperature | ISO 306/B50 | 142 | °C | |
| 玻璃转化温度 | ISO 11357-2 | 142 | °C | |
| Linear coefficient of thermal expansion | MD | ISO 11359-2 | 7E-05 | cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | MD2.0mm | ISO 294-4 | 0.70 | % |
| TD2.0mm | ISO 294-4 | 0.65 | % | |
| Water absorption rate | (23°C,24hr) | ISO 62 | 0.30 | % |
| (23°C,50RH) | ISO 62 | 0.12 | % | |
| melt mass-flow rate | 300℃/1.2Kg | ISO 1133 | 33.0 | cm3/10min |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Volume resistivity | IEC 60093 | 1E+16 | Ω.cm | |
| Surface resistivity | IEC 60093 | 1E+16 | Ω.cm | |
| Dielectric strength | IEC 60243-1 | 34 | KV/mm | |
| Dielectric constant | 23°C | IEC 60250 | 3.00 | 1MHz |
| Dissipation factor | 23°C | IEC 60250 | 1E-03 | 100HZ |
| 23°C | IEC 60250 | 0.01 | 1MHz | |
| 相对漏电起痕指数 | IEC 60112 | 250 | V | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Ball Pressure Test | ISO 2039-1 | 114 | Mpa | |
| flame retardant performance | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | UL -94 | V-2 | 0.75mm | |
| UL -94 | V-2 | 1.00mm | ||
| UL -94 | V-2 | 1.50mm | ||
| UL -94 | V-2 | 3.00mm | ||
| Extreme Oxygen Index | ISO 4589-2 | 30 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.