| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179 | 13 kJ/m² |
| flammability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| UL flame retardant rating | 2.0mm | UL 94 | V-0 |
| 3.0mm | UL 94 | 5VA |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | Yield,23°C | ISO 527-2 | 39.0 MPa |
| Bending modulus | 23°C | ISO 178 | 2200 MPa |
| bending strength | 23°C | ISO 178 | 67.0 MPa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 85.0 °C |
| Linear coefficient of thermal expansion | MD:23to80°C | JISK7197 | 8E-05 cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Melt Volume Flow Rate (MVR) | 200°C/5.0kg | ISO 1133 | 1.30 cm³/10min |
| Shrinkage rate | Internal Method | 0.40to0.60 % | |
| density | 23°C | ISO 1183 | 1.19 g/cm³ |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Rockwell hardness | R-Sale,23°C | ISO 2039-2 | 109 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.