Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate | | ASTMD570 | 0.30 % |
density | | ASTMD792 | 1.22 g/cm³ |
Shrinkage rate | | ASTMD955 | 0.80 % |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | R-Scale | ASTMD785 | 113 |
| | ASTMD2240 | 80 |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ASTMD638 | 207 MPa |
tensile strength | Yield | ASTMD638 | 48.3 MPa |
elongation | Break | ASTMD638 | 380 % |
Flexural modulus | | ASTMD790 | 345 MPa |
bending strength | Yield | ASTMD790 | 55.2 MPa |
compressive strength | | ASTMD695 | 27.6 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 无断裂 |
Suspended wall beam without notch impact strength | | ASTMD4812 | 无断裂 |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Volume resistivity | | ASTMD257 | 1E+12 ohms·cm |
dielectric strength | | ASTMD149 | 20 kV/mm |
dielectric constant | | ASTMD150 | 5.10 |
Dissipation Factor | | ASTMD150 | 0.10 |
arc resistance | | ASTMD495 | 122 sec |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD696 | 2.2E-05 cm/cm/°C |
thermal conductivity | | ASTMC177 | 0.23 W/m/K |
| | ASTMD648 | 87.8 °C |
| | ASTMD648 | 54.4 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.