Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Resistance to environmental stress cracking | | ASTMD1693B | 25.0 hr |
density | | ASTMD1505 | 0.953 g/cm³ |
melt mass-flow rate | | ASTMD1238 | 0.23 g/10min |
melt mass-flow rate | | ASTMD1238 | 26 g/10min |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
BlowMoldingBarrelTemperature | | | 170到190 °C |
BlowMoldingDieTemperature | | | 175到190 °C |
Blow molding temperature | | | 170到200 °C |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile stress | Yield | ISO527-2/2 | 30.0 MPa |
Tensile strain | Break | ISO527-2/2 | >900 % |
Flexural modulus | | ISO178 | 1000 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Charpy Notched Impact Strength | | ASTMD256 | 9.0 kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD2117 | 130 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.