TPU-Ester 890 AN BASF GERMANY

0

Technical Data Sheet

elastomerTest ConditionTest MethodTest Result
tear strengthASTM D624144 kN/m
elongationBreakASTM D412480 %
tensile strengthASTM D41239.3 MPa
tensile strength300%StrainASTM D41231.0 MPa
tensile strength100%StrainASTM D41213.8 MPa
Permanent compression deformation70°C,22hrASTM D395B45 %
Permanent compression deformation23°C,22hrASTM D395B20 %
mechanical propertiesTest ConditionTest MethodTest Result
Wear resistanceDIN 5351625 mm³
Taber abraserASTM D104445.0 mg
Bending modulusInjectionASTM D79066.9 MPa
Tensile modulusInjectionASTM D41229.0 MPa
thermal performanceTest ConditionTest MethodTest Result
Vicat softening temperatureInternal Method81 °C
Vicat softening temperatureASTM D1525120 °C
Glass transition temperatureInternal Method-14.0 °C
Physical propertiesTest ConditionTest MethodTest Result
melt mass-flow rate190°C/8.7kgASTM D123815to30 g/10min
densityASTM D7921.22 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardnessShoreAASTM D224092
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.