physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate | | ISO62 | 0.22 % |
Shrinkage rate | | ISO294-4 | 0.40到0.70 % |
Water absorption rate | | ISO62 | 0.70 % |
density | | ISO1183 | 1.15 g/cm³ |
melt mass-flow rate | | ISO1133 | 15 g/10min |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | HB |
UL flame retardant rating | | UL94 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ISO527-2/1 | 2100 MPa |
Tensile stress | Yield | ISO527-2/50 | 50.0 MPa |
Flexural modulus | | ISO178 | 2200 MPa |
Bending stress | | ISO178 | 66.0 MPa |
Tensile stress | | ISO527-2 | 63.0 MPa |
Tensile stress | | ISO527-2 | 20.0 MPa |
Tensile strain | Yield | ISO527-2/50 | 4.3 % |
Tensile strain | | ISO527-2 | 6.3 % |
Tensile strain | Break | ISO527-2 | 35 % |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Charpy Notched Impact Strength | | ISO179/1eA | 44 kJ/m² |
Impact strength of simply supported beam without notch | | ISO179/1eU | 无断裂 |
Impact strength of cantilever beam gap | | ISO180/1A | 45 kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ISO75-2/B | 121 °C |
| | ISO75-2/Ae | 100 °C |
vicat | | ISO306/B50 | 120 °C |
| | ISO11359-2 | 9.5E-04 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.