Rubber Techsil® RTV27941

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
density1.10 g/cm³
Shrinkage rate0.10 %
thermosettingTest ConditionTest MethodTest Result
stripping time1400 min
Uncured PropertiesTest ConditionTest MethodTest Result
colourTranslucent
colourTranslucent
MixRatiobyWeight(PBW)10
MixRatiobyWeight(PBW)1.0
1.5 Pa·s
45 Pa·s
24 hr
90 min
Cured PropertiesTest ConditionTest MethodTest Result
Supporting hardness41
tensile strength6.40 MPa
elongationBreak360 %
tear strength20.0 kN/m
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.