TPU IROGRAN® A 80 P 4926DP HUNTSMAN GERMANY
7
Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Permanent compression deformation | 70℃,24h | 42 % | |
| 23℃,24h | ASTM D395 | 24 % | |
| tear strength | ASTM D624 | 73.6 kN/m | |
| elongation | Break | ASTM D412 | 650 % |
| tensile strength | Break | ASTM D412 | 31.7 Mpa |
| 300%Strain | 6.21 Mpa | ||
| 100%Strain | ASTM D412 | 4.14 Mpa | |
| Shore hardness | ShoreD | 31 | |
| ShoreA | ASTM D2240 | 80 |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Melting temperature | 127-154 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shrinkage rate | MD | 0.8 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.