Unspecified Starpylen MF004S EUROSTAR FRANCE
Properties:
Filler glass fiber reinforced material 20% filler by weight
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | Filler | glass fiber reinforced material | 20% | filler by weight |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 8.0 | kJ/m² |
| Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 35 | kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| elongation | Yield | ASTM D638 | 3.1 | % |
| Bending modulus | ISO 178 | 4100 | MPa | |
| bending strength | ISO 178 | 102 | MPa | |
| Tensile modulus | ISO 527-2/1 | 4700 | MPa | |
| tensile strength | Yield | ISO 527-2/50 | 78.0 | MPa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8MPa,Unannealed,64.0mmSpan | ISO 75-2/Af | 131 | °C |
| Linear coefficient of thermal expansion | MD:23to60°C | ISO 11359-2 | 4.4E-05 | cm/cm/°C |
| TD:23to60°C | ISO 11359-2 | 1.3E-04 | cm/cm/°C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ISO 1183 | 1.05 | g/cm³ | |
| Shrinkage rate | MD:4.00mm | Internal Method | 0.30to0.50 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.