Rubber Shin-Etsu Elastomer KE-5006U

0

Technical Data Sheet

thermosettingTest ConditionTest MethodTest Result
Post curing time4.0 hr
physical property Test ConditionTest MethodTest Result
density1.18 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardness55
Supplementary InformationTest ConditionTest MethodTest Result
CureAgentDCBP
elastomerTest ConditionTest MethodTest Result
compression set33 %
tensile strength 11.0 MPa
elongationBreak500 %
tear strength32.4 kN/m
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.