PES JFL-4036 SABIC INNOVATIVE US

117

Form:Granules | Grade:Injection grade

Properties:
High temperature creep reDimensional stability
Typical Applications:
Electronic fieldmechanicalBearing retainer
Product Description
Certificates(0)
Datasheet

Product Description

Typical Applications:Electronic field | mechanical | Bearing retainer
Properties:High temperature creep re | Dimensional stability

Certificates

No Data...

Technical Data Sheet

impact performanceTest ConditionTest MethodTest ResultTest Unit
Suspended wall beam without notch impact strength23°C3ISO 180/1U24kJ/m²
Suspended wall beam without notch impact strength23°CASTM D4812360J/m
Dart impact23°C,EnergyatPeakLoadASTM D37639.40J
Dart impact--ISO 6603-22.47J
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
Wear factorWasherASTM D3702Modified60.010^-10in^5-min/ft-lb-hr
Friction coefficientStaticASTM D3702Modified0.36
Friction coefficientDynamicASTM D3702Modified0.46
bending strength--ISO 178138Mpa
elongationBreakASTM D6381.9%
tensile strengthBreakISO 527-289.0Mpa
tensile strengthBreakASTM D638129Mpa
Tensile modulus--ISO 527-2/19540Mpa
Tensile modulus--2ASTM D63810200Mpa
bending strength--ASTM D790179Mpa
Bending modulus--ISO 17810800Mpa
Bending modulus--ASTM D7909930Mpa
elongationBreakISO 527-21.5%
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Linear coefficient of thermal expansionTD:-40to40°CASTME8313.5E-05cm/cm/°C
Linear coefficient of thermal expansionMD:-40to40°CASTME8312.3E-05cm/cm/°C
Hot deformation temperature1.8MPa,Unannealed,64.0mmSpan4ISO 75-2/Af210°C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTM D648208°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
Water absorption rateEquilibrium,23°C,50%RHISO 620.50%
Water absorption rate24hr,50%RHASTM D5700.29%
Shrinkage rateMD:24hrISO 294-40.10-0.30%
Shrinkage rateTD:24hrISO 294-40.30-0.60%
Shrinkage rateTD:24hrASTM D9550.30-0.60%
Shrinkage rateMD:24hrASTM D9550.10-0.40%
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.

Sourcing & Prices

Selling & Verification

Explore Materials

Price Index

+86 0755 27873515

Room 906, Global Digital Building, No. 9 Gaoxin Middle 3rd Road, Maling Community, Yuehai Subdistrict, Nanshan District, Shenzhen, Guangdong Province, China