Share
Add to compare

PBT 310-1001 SABIC INNOVATIVE JAPAN

32

Form:Granules | Grade:Injection grade

Properties:
High rigidityGlass fiber reinforced
Typical Applications:
Electrical applicationsAutomotive Applicationscurrency
Product Description
Certificates(1)
Datasheet

Product Description

Typical Applications:Electrical applications | Automotive Applications | currency
Properties:High rigidity | Glass fiber reinforced

Certificates

UL
UL

Technical Data Sheet

impact performanceTest ConditionTest MethodTest ResultTest Unit
Dart impact23°C6ASTM D302940.7J
Dart impact23°CASTM D302940.7J
flammabilityTest ConditionTest MethodTest ResultTest Unit
UL flame retardant rating1.5mmUL 94HB
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
bending strengthBreak,50.0mmSpanASTM D79082.7Mpa
bending strengthYield,50.0mmSpanASTM D79082.7Mpa
Bending modulus50.0mmSpanASTM D7902340Mpa
elongationBreakASTM D638300%
tensile strengthBreakASTM D63851.7Mpa
tensile strengthYieldASTM D63851.7Mpa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Hot deformation temperature0.45MPa,Unannealed,6.40mmASTM D648154°C
Hot deformation temperature1.8MPa,Unannealed,6.40mmASTM D64854.4°C
Linear coefficient of thermal expansionMD:-40to40°CASTME8318.1E-05cm/cm/°C
Linear coefficient of thermal expansionMD:60to138°CASTME8311.4E-04cm/cm/°C
RTI ElecUL 746120°C
RTI ImpUL 746120°C
RTI StrUL 746140°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
Melt viscosityInternal Method600Pa·s
Water absorption rate24hrASTM D5700.080%
Shrinkage rateTD:--3Internal Method1.6-2.4%
Shrinkage rateTD:--2Internal Method1.0-1.7%
Shrinkage rateMD:--3Internal Method1.5-2.3%
Shrinkage rateMD:--2Internal Method0.90-1.6%
Specific volumeASTM D7920.770cm³/g
Electrical performanceTest ConditionTest MethodTest ResultTest Unit
High voltage arc tracing rateHVTRUL 746PLC 1
Compared to the anti leakage trace indexCTIUL 746PLC 0
Arc resistanceASTM D495PLC 5
Dissipation factor1MHzASTM D1500.020
Dissipation factor100HzASTM D1502E-03
Dielectric constant1MHzASTM D1503.10
Dielectric constant100HzASTM D1503.30
Volume resistivityASTM D257>4.0E+16ohms·cm
Dielectric strength1.60mm,inAirASTM D14923KV/mm
Dielectric strength1.60mm,in OilASTM D14923KV/mm
Dielectric strength3.20mm,inAirASTM D14916KV/mm
Dielectric strength3.20mm,in OilASTM D14916KV/mm
hardnessTest ConditionTest MethodTest ResultTest Unit
Rockwell hardnessR-ScaleASTM D785117
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.