Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA3 | 18.0 | kJ/m² |
| 23°C | NoBreak | |||
| -30°C | NoBreak | |||
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Normal combustion performance with a thickness of 1.6mm | 1.50mm,UL | J | HB | |
| Burning rate | 2.00mm | ISO 3795 | 60 | mm/min |
| UL flame retardant rating | 1.5mm | UL 94 | HB | |
| 3.0mm | UL 94 | HB | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | Break | ASTM D638 | 35.0 | Mpa |
| elongation | Yield | ASTM D638 | 2.7 | % |
| Tensile strain | Yield,3.20mm,Injection | ISO 527-2/50 | 2.5 | % |
| Yield,3.20mm,Injection | ISO 527-2/100 | 2.6 | % | |
| elongation | Break | ASTM D638 | 8.7 | % |
| Nominal fracture strain | ISO 527-23 | 20 | % | |
| Bending modulus | ASTM D790 | 2480 | Mpa | |
| 3.20mm,InjectionMolded | ISO 178 | 2400 | Mpa | |
| bending strength | ASTM D790 | 75.0 | Mpa | |
| 3.20mm,InjectionMolded | ISO 178 | 70.0 | Mpa | |
| Tensile modulus | 3.20mm,Injection | ISO 527-2 | 2340 | Mpa |
| ISO 527-23 | 2400 | Mpa | ||
| tensile strength | Yield | ASTM D638 | 48.0 | Mpa |
| Yield,3.20mm,Injection | ISO 527-2/50 | 45.0 | Mpa | |
| Yield,3.20mm,Injection | ISO 527-2/100 | 47.0 | Mpa | |
| Yield | ISO 527-23 | 48.0 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 0.45MPa,Unannealed | ASTM D648 | 87.0 | °C |
| 1.8MPa,Unannealed | ASTM D648 | 74.0 | °C | |
| 1.8MPa,Annealed | ISO 75-2/A | 95.0 | °C | |
| 1.8MPa | ISO 75-23 | 95.0 | °C | |
| Vicat softening temperature | ASTM D15258 | 99.0 | °C | |
| ISO 306/B50 | 95.0 | °C | ||
| 50N | ISO 3063 | 92.0 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Apparent density | ISO 60 | 0.65 | g/cm³ | |
| melt mass-flow rate | 220°C/10.0kg | ASTM D1238 | 28 | g/10min |
| 230°C/3.8kg | ASTM D1238 | 8.0 | g/10min | |
| 220°C/10.0kg | ISO 1133 | 28 | g/10min | |
| Melt Volume Flow Rate (MVR) | 220°C/10.0kg | IEC 60093 | 27.0 | cm3/10min |
| Shrinkage rate | MD | ASTM D955 | 0.40-0.70 | % |
| MD | ISO 294-4 | 0.40-0.70 | % | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Scale | ASTM D785 | 108 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.