impact performanceTest ConditionTest MethodTest ResultTest Unit
Impact strength of cantilever beam gapASTM D256A44to48J/m
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
Poisson's ratioASTM D6380.43
bending strengthASTM D79024.0to30.0MPa
Bending modulusASTM D790768to900MPa
elongationYieldASTM D63825to30%
tensile strengthASTM D63817.0to20.0MPa
Tensile modulusASTM D638553to850MPa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Linear coefficient of thermal expansionMD:100to150°CASTME8311.4E-04cm/cm/°C
Linear coefficient of thermal expansionMD:50to100°CASTME8311.8E-04cm/cm/°C
Linear coefficient of thermal expansionMD:0to50°CASTME8311.5E-04cm/cm/°C
Linear coefficient of thermal expansionMD:-40to0°CASTME8319.7E-05cm/cm/°C
Glass transition temperatureASTME154557.0to60.0°C
Hot deformation temperature1.8MPa,UnannealedASTM D64836.0to38.0°C
Hot deformation temperature0.45MPa,UnannealedASTM D64847.0to50.0°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
viscosity30°C475mPa·s
Water absorption rateEquilibriumASTM D5700.93%
density1.13g/cm³
Electrical performanceTest ConditionTest MethodTest ResultTest Unit
Dielectric constant1kHzASTM D1504.66
Dielectric constant60HzASTM D1505.33
Dielectric strengthASTM D14914kV/mm
Dielectric constant1MHzASTM D1503.94
hardnessTest ConditionTest MethodTest ResultTest Unit
Shore hardnessShoreDASTM D224070to74
Supplementary InformationTest ConditionTest MethodTest ResultTest Unit
CriticalExposure15.0mJ/cm²
Puncture intensity137.2µm
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.