PBT/ASA 9KY22130 HUV
0
- Properties:Fillerreinforcement materialglass fiber reinforcement material30%filler by weight additiveheat stabilizerUV stabilizercharacteristicsgood UV resistancethermal stability
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 1.55 g/cm³ | |
Shrinkage rate | 0.70 % | ||
Water absorption rate | ISO 62 | 0.10 % |
other | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL 94 | HB | |
UL 94 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile stress | ISO 527-2/5 | 120 MPa | |
Tensile strain | ISO 527-2/5 | 2.5 % | |
Impact strength of cantilever beam gap | ISO 180/1A | 9.0 kJ/m² | |
Tensile modulus | ISO 527-2/5 | 9500 MPa | |
Impact strength of cantilever beam gap | ISO 180/1A | 11.0 kJ/m² |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Surface Resistivity | IEC 60093 | 1E+14 ohms | |
Volume resistivity | IEC 60093 | 1E+16 ohms·cm |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
ISO 75-2/B | 210 °C | ||
ISO 75-2/A | 155 °C | ||
melting temperature | ISO 11357 | 225 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.