PA66 9A34100 H 4Plas
Properties:
Characteristics high fluidity thermal stability
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | Characteristics | high fluidity | thermal stability |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | -30°C | ISO 180/1A | 10 | kJ/m² |
| -20°C | ISO 180/1A | 10 | kJ/m² | |
| 23°C | ISO 180/1A | 14 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.6mm | UL 94 | HB | |
| 3.2mm | UL 94 | HB | ||
| Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 650 | °C |
| UL flame retardant rating | 0.0295 in | UL 94 | HB | |
| 0.0630 in | UL 94 | HB | ||
| Burning wire flammability index | 0.0787 in | IEC 60695-2-12 | 1200 | °F |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | 73°F | ISO 527-2/5 | 290000 | psi |
| 23°C | ISO 527-2/5 | 2000 | MPa | |
| tensile strength | Break,23°C | ISO 527-2/5 | 65.0 | MPa |
| Tensile strain | Break,23°C | ISO 527-2/5 | 5.0 | % |
| tensile strength | Break, 73°F | ISO 527-2/5 | 9430 | psi |
| Tensile strain | Break,73°F | ISO 527-2/5 | 5.0 | % |
| Impact strength of cantilever beam gap | -22°F | ISO 180/1A | 4.8 | ft·lb/in² |
| -4°F | ISO 180/1A | 4.8 | ft·lb/in² | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 80.0 | °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 60.0 | °C | |
| Vicat softening temperature | ISO 306/B | 240 | °C | |
| Melting temperature | ISO 11357 | 262 | °C | |
| ISO 11357 | 504 | °F | ||
| Hot deformation temperature | 66 psi, Unannealed | ISO 75-2/B | 176 | °F |
| 264 psi, Unannealed | ISO 75-2/A | 140 | °F | |
| Vicat softening temperature | ISO 306/B | 464 | °F | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ISO 1183 | 1.10 | g/cm³ | |
| Water absorption rate | Equilibrium, 73°F, 50% RH | ISO 62 | 2.2 | % |
| density | ISO 1183 | 1.10 | g/cm³ | |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 2.2 | % |
| water content | ISO 960 | <2000 | ppm | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | IEC 60093 | 1E+13 | ohms | |
| Volume resistivity | IEC 60093 | 1E+15 | ohms·cm | |
| Compared to the anti leakage trace index | IEC 60112 | PLC 0 | ||
| Surface resistivity | IEC 60093 | 1E+13 | ohms | |
| Volume resistivity | IEC 60093 | 1E+15 | ohms·cm | |
| Compared to the anti leakage trace index | IEC 60112 | PLC 0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.