TPEE TX633

66
  • Properties:
    High resilience
    High impact
    High tensile strength
    Good softness
    Aging resistance
    High temperature resistan
    Low temperature resistanc
  • Usages:
    cable
    film
    Spinning products
    Automotive sector
    Electric wire
    Cable

Technical Data Sheet

otherTest ConditionTest MethodTest Result
notes粘度; 1.100 ± 0.025
processabilityTest ConditionTest MethodTest Result
Dry conditions110
Mechanical propertiesTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTM D256/ISO 17925 kg·cm/cm(J/M)ft·lb/in
elongation at breakASTM D412/ISO 527>400 %
tensile strength ASTM D412/ISO 52730 kg/cm²(MPa)[Lb/in²]
Rockwell hardnessASTM D78563D
Physical propertiesTest ConditionTest MethodTest Result
densityASTM D9551.26 %
melt mass-flow rateASTM D1238/ISO 113330 g/10min
Thermal performanceTest ConditionTest MethodTest Result
melting temperature214 ± 2.0 ℃(℉)
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.