optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Haze ratio | ASTMD1003 | 6.0 % |
film | Test Condition | Test Method | Test Result |
---|---|---|---|
Film thickness - tested | 19 µm | ||
Secant modulus | ASTMD882 | 2760 MPa | |
ASTMD882 | 2550 MPa | ||
tensile strength | ASTMD882 | 331 MPa | |
ASTMD882 | 82.7 MPa | ||
elongation | ASTMD882 | 60 % | |
ASTMD882 | 340 % | ||
Elmondov tear strength | ASTMD1922 | 40 g | |
ASTMD1922 | 100 g |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.