PPO 731S-701S SABIC INNOVATIVE SHANGHAI
273
Form:Granules | Grade:Injection grade
Properties:
High mobilityAntistaticHigh temperature resistancurrency
Typical Applications:
Food containers
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Food containers |
| Properties: | High mobility | Antistatic | High temperature resistan | currency |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 15 | kJ/m² |
| -30°C | ISO 180/1A | 5.0 | kJ/m² | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 15 | kJ/m² |
| -30°C | ISO 179/1eA | 5.0 | kJ/m² | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| bending strength | ISO 178 | 75.0 | Mpa | |
| Bending modulus | ISO 178 | 2200 | Mpa | |
| Tensile strain | Break | ISO 527-2/50 | 30 | % |
| Yield | ISO 527-2/50 | 5.0 | % | |
| tensile strength | Break | ISO 527-2/50 | 50.0 | Mpa |
| Yield | ISO 527-2/50 | 55.0 | Mpa | |
| Tensile modulus | ISO 527-2/1 | 2300 | Mpa | |
| injection | Test Condition | Test Method | Test Result | Test Unit |
| Temperature at the front of the material cylinder | 280 to 300 | °C | ||
| Spray nozzle temperature | 260 to 280 | °C | ||
| Processing (melt) temperature | 280 to 300 | °C | ||
| Mold temperature | 80 to 120 | °C | ||
| Temperature in the middle of the barrel | 260 to 280 | °C | ||
| Temperature at the rear of the barrel | 240 to 260 | °C | ||
| Hopper temperature | 60 to 80 | °C | ||
| drying time | 2.0 to 3.0 | hr | ||
| drying temperature | 100 to 120 | °C | ||
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | Across Flow : 23 to 80°C | ISO 11359-2 | 7.0E-5 | cm/cm/°C |
| Flow : 23 to 80°C | ISO 11359-2 | 7.0E-5 | cm/cm/°C | |
| Vicat softening temperature | -- | ISO 306/B120 | 140 | °C |
| -- | ISO 306/B50 | 135 | °C | |
| Hot deformation temperature | 1.8 MPa, Unannealed, 4.00 mm, 100 mm Span | ISO 75-2/Ae | 115 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 0.060 | % |
| Saturation, 23°C | ISO 62 | 0.23 | % | |
| Melt Volume Flow Rate (MVR) | 280°C/5.0 kg | ISO 1133 | 8.00 | cm3/10min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.