PP Moplen  CA60A LYONDELLBASELL SAUDI

26
  • Properties:
    Low hardnessHigh mobilityHigh flexibilityEasy to processHigh impact resistanceGood flexibility
  • Usages:
    Industrial applications
  • Compare View Prices

Technical Data Sheet

Basic PerformanceTest ConditionTest MethodTest Result
densityMethod AISO 11830.888 Method A
melt mass-flow rate230°C/2.16 kgISO 113314 g/10min
mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthYieldISO 527-16 Mpa
tensile strengthBreak 23℃ISO 527-120 Mpa
Tensile strainBreakISO 527-1>500 %
Bending modulusISO 17880 Mpa
Shore hardnessShore DISO 86830
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature0.45Mpa, UnannealedISO 75B-144 °C
Vicat softening temperatureA50 (50°C/h 10N)ISO 30656 °C
Melting temperature142 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.