Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate | | ISO62 | <0.50 % |
density | | ISO1183 | 1.90 g/cm³ |
Shrinkage rate | | ISO2577 | 0.020 % |
Shrinkage rate | | DIN53464 | 0.0 % |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | Compression Molded | ISO527-2 | 12000 MPa |
Tensile stress | | ISO527-2 | 86.0 MPa |
Tensile strain | | ISO527-2 | 1.5 % |
Flexural modulus | Compression Molded | ISO178 | 10000 MPa |
Bending stress | Compression Molded | ISO178 | 182 MPa |
compression stress | | ISO14126 | 90.0 MPa |
Poisson's ratio | | 内部方法 | 0.30 |
MatrixCrazingStrain | | 内部方法 | 0.40 % |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Charpy Notched Impact Strength | Compression Molded | ISO179 | 82 kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ISO75-2/A | >200 °C |
Continuous use temperature | | 内部方法 | 165 °C |
Glass Transition Temperature | | DSC | 170 °C |
| | ISO11359-2 | 1E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.