HDPE Hoegolen® AIM GF10 blue 5117 HP-T H?glmeier Polymer-Tech GmbH & Co. KG
Properties:
Filler glass fiber reinforced material
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | Filler | glass fiber reinforced material |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179 | 13 | kJ/m² |
| Impact strength of simply supported beam without notch | -23°C | ISO 179 | 78 | kJ/m² |
| 23°C | ISO 179 | 150 | kJ/m² | |
| Charpy Notched Impact Strength | -23°C | ISO 179 | 9.0 | kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | ISO 527-2 | 1400 | MPa | |
| tensile strength | Break | ISO 527-2 | 11.0 | MPa |
| -- | ISO 527-2 | 24.0 | MPa | |
| Tensile strain | Break | ISO 527-2 | 37 | % |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | ISO 306/A50 | 124 | °C | |
| Crystallization peak temperature | DSC | ISO 3146 | 143 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | 23°C | DIN 53479 | 1.01 | g/cm³ |
| melt mass-flow rate | 190°C/21.6kg | ISO 1133 | 12 | g/10min |
| ash content | DIN EN60 | 12 | % | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Ball Pressure Test | H132/30 | DIN 53435 | 39.0 | MPa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.