Share
Add to Compare

Polyester PELPRENE™ P48U TOYOBO CO., LTD.

Product Description
Certificates(0)
Datasheet

Product Description

Certificates

No Data...

Technical Data Sheet

impact performanceTest ConditionTest MethodTest ResultTest Unit
Impact strength of cantilever beam gapASTM D256无断裂
flammabilityTest ConditionTest MethodTest ResultTest Unit
UL flame retardant ratingUL 94HB
elastomerTest ConditionTest MethodTest ResultTest Unit
Permanent compression deformationJISK630151%
tear strengthASTM D624103kN/m
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
Bending modulusASTM D79063.0MPa
elongationBreakASTM D638700%
tensile strength50%StrainASTM D6388.30MPa
tensile strength--ASTM D63826.0MPa
Taber abraser1000CyclesASTM D104417.0mg
compressive strength10%StrainASTM D6956.10MPa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Linear coefficient of thermal expansionMDASTME8311.7E-04cm/cm/°C
Melting temperatureDSC176°C
Vicat softening temperatureASTM D1525130°C
Brittle temperatureJISK6301<-65.0°C
Hot deformation temperature1.8MPa,UnannealedASTM D648<25.0°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
Water absorption rateEquilibrium,23°C,65%RHASTM D5700.47%
Shrinkage rateMD:2.00mmASTM D9550.60%
melt mass-flow rate230°C/2.16kgASTM D123825g/10min
densityASTM D7921.14g/cm³
Electrical performanceTest ConditionTest MethodTest ResultTest Unit
Dielectric strengthJISK211122kV/mm
Volume resistivityASTM D2574E+12ohms·cm
hardnessTest ConditionTest MethodTest ResultTest Unit
Shore hardnessShoreDASTM D224041
Shore hardnessShoreAJISK630192
Supplementary InformationTest ConditionTest MethodTest ResultTest Unit
ResilienceJISK630176%
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.