Product Description
| Typical Applications: | Food service sector | Soft packaging composite materials Liquid packagin |
| Properties: | Resistance to stress crac | High toughness | Heat sealing performance |
Certificates
No Data...
Technical Data Sheet
| Other performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Water vapor permeability | 38℃,90% RH | DIN 53122/2 | 0.41 | g·mm/m2/atm/24hr |
| Starting temperature of heat sealing | Internal Method | 85 | ℃ | |
| Basic Performance | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | 190℃/2.16kg | ISO 1133 | 11 | g/10min |
| 190℃/2.16kg | ASTM D-1238 | 11 | g/10min | |
| Monomer content | Internal Method | 9.7 | % | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| elongation | Break,Compression Molded | ASTMD638 | 600 | % |
| Elongation at Break | Compression Molded | ISO 527-2 | 600 | % |
| Compression Molded | ASTM D-638 | 600 | % | |
| tensile strength | Compression Molded,Break | ISO 527-2 | 17.6 | MPa |
| Compression Molded,Break | ASTM D-638 | 17.6 | MPa | |
| Yield,Compression Molded | ISO 527-2 | 7.93 | MPa | |
| Yield,Compression Molded | ASTM D-638 | 7.93 | MPa | |
| Break,Compression Molded | ASTMD638 | 17.6 | Mpa | |
| Yield,Compression Molded | ASTMD638 | 7.93 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | ASTMD1525 | 81.1 | °C | |
| Melting temperature | Internal Method | 97.8 | °C | |
| Vicat softening temperature | ASTM D-1525 | 81.1 | ℃ | |
| Melting temperature | Internal Method | 97.8 | ℃ | |
| Vicat softening temperature | ISO 306 | 81.1 | ℃ | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ISO 1183 | 0.938 | g/cm³ | |
| ASTM D-792 | 0.938 | g/cm³ | ||
| Content of comonomer | Internal Method | 9.7 | % | |
| melt mass-flow rate | 190°C/2.16kg | ASTMD1238 | 11 | g/10min |
| density | ASTMD792 | 0.938 | g/cm³ | |
| film | Test Condition | Test Method | Test Result | Test Unit |
| Water vapor permeability | 38°C,90%RH | DIN 53122/2 | 0.41 | g·mm/m²/atm/24hr |
| Initial sealing temperature | Internal Method | 85.0 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.