physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Shrinkage rate | ASTM D-955 | 0.2-0.6 % | |
Haze ratio | ASTM D-1003 | 1.3 | |
transmittance | ASTM D-1003 | 89 % | |
refractive index | ASTM D-542 | 1.57 % |
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Water absorption rate | ASTM D-570 | 0.1 % | |
melt mass-flow rate | ASTM D-1238 | 4.2 g/10min | |
density | ASTM D-792 | 1.04 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Rockwell hardness | ASTM D-785 | R-68 R scale | |
elongation at break | ASTM D-638 | 65 % | |
Tensile modulus | ASTM D-638 | 21800 kg/cm2 | |
Flexural modulus | ASTM D-790 | 21800 kg/cm2 | |
Subduing tensile strength | ASTM D-638 | 286 kg/cm2 | |
Impact strength of cantilever beam gap | ASTM D-256 | 10.2 kg.cm/cm | |
bending strength | ASTM D-790 | 530 kg/cm2 |
Other performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Compliant with FDA standards | Yes | ||
medical grade | Yes |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
vicat | ASTM D-1525 | 97 Deg.C | |
Heat distortion temperature | ASTM D-648 | 85 Deg.C | |
burning rate | UL 94 | 94HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.