PETG K2012 SK KOREA
742
Form:Granules | Grade:Extrusion grade
Properties:
Easy to processAntichemicalHigh toughnessHigh gloss
Typical Applications:
sheetchipfilmcontainerbottleToy
Product Description
Certificates(2)
Datasheet
Product Description
| Typical Applications: | sheet | chip | film | container | bottle | Toy |
| Properties: | Easy to process | Antichemical | High toughness | High gloss |
Certificates
TDS
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Refractive index | ASTM D542/ISO 489 | 1.570 | ||
| Transmittance rate | ASTM D1003/ISO 13468 | 89.0 | % | |
| gloss | 60° | ASTME308 | 159 | |
| Refractive index | ASTM D542 | 1.570 | ||
| transmissivity | ASTM D1003 | 89.0 | % | |
| turbidity | ASTM D1003 | <1.0 | % | |
| other | Test Condition | Test Method | Test Result | Test Unit |
| purpose | 电气/电子应用领域.护罩.玩具.片材.瓶子.医疗/护理领域 | |||
| Color | GT | |||
| characteristic | 高光泽.耐化学.食品级.韧性良好.可加工性良好 | |||
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.0mm | UL 94 | HB | |
| 1.5mm | UL 94 | HB | ||
| 3.0mm | UL 94 | V-2 | ||
| Basic Performance | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D-792 | 1.27 | g/cm³ | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Impact strength of cantilever beam gap | ASTM D-256 | 100 | J/m | |
| elongation | ASTM D-638 | 140 | % | |
| bending strength | ASTM D-790 | 73 | Mpa | |
| Bending modulus | ASTM D-790 | 2100 | Mpa | |
| Tensile strength (fracture) | ASTM D-638 | 28 | Mpa | |
| tensile strength | Yield | ASTM D-638 | 50 | Mpa |
| bending strength | ASTM D790/ISO 178 | 80 | kg/cm²(MPa)[Lb/in²] | |
| Bending modulus | ASTM D790/ISO 178 | 2150 | kg/cm²(MPa)[Lb/in²] | |
| Rockwell hardness | ASTM D785 | 116 | kg·cm/cm(J/M)ft·lb/in | |
| Elongation at Break | ASTM D412/ISO 527 | 70 | % | |
| Bending modulus | ASTM D790 | 2150 | Mpa | |
| bending strength | ASTM D790 | 80.0 | Mpa | |
| tensile strength | Yield | ASTM D638 | 53.0 | Mpa |
| Break | ASTM D638 | 26.0 | Mpa | |
| elongation | Yield | ASTM D638 | 5.0 | % |
| Break | ASTM D638 | 70 | % | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | HDT | ASTM D-648 | 70 | °C |
| 0.45MPa,Unannealed | ASTM D648 | 74.0 | °C | |
| 1.8MPa,Unannealed | ASTM D648 | 70.0 | °C | |
| Vicat softening temperature | ASTM D15256 | 83.0 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | ASTM D-570 | 0.2 | % | |
| Shrinkage rate | ASTM D-955 | 0.30-0.60 | % | |
| ASTM D955 | 0.2 | % | ||
| density | ASTM D792/ISO 1183 | 1.27 | ||
| Water absorption rate | 24hr | ASTM D570 | 0.20 | % |
| Color B | ASTME308 | <1.00 | ||
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dissipation factor | 1MHz | ASTM D150 | 0.023 | |
| 1kHz | ASTM D150 | 5E-03 | ||
| Dielectric constant | 1MHz | ASTM D150 | 2.40 | |
| Surface resistivity | ASTM D257 | 1E+16 | ohms | |
| Volume resistivity | ASTM D257 | 1E+15 | ohms·cm | |
| Dielectric strength | ASTM D149 | 16 | KV/mm | |
| Dielectric constant | 1kHz | ASTM D150 | 2.60 | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Scale | ASTM D785 | 116 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.