Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.31 g/cm³ |
Shrinkage rate | | ASTMD995 | 0.4 % |
Shrinkage rate | | ASTMD995 | 0.6 % |
Shrinkage rate | | | 86.4 cm |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ASTMD638 | 2410 MPa |
bending strength | | ASTMD790 | 69.6 MPa |
Flexural modulus | | ASTMD790 | 2620 MPa |
Impact strength of cantilever beam gap | | ASTMD256 | 801 J/m |
Impact strength of cantilever beam gap | | ASTMD256A | 107 J/m |
tensile strength | | ASTMD638 | 41.4 MPa |
Other performance | Test Condition | Test Method | Test Result |
---|
Regional availability | | | 非洲和中东,亚太地区,欧洲,北美,南美 |
Flame retardant performance | Test Condition | Test Method | Test Result |
---|
fire rating | | UL-94 | 1.50mm V-0,5VA |
fire rating | | UL-94 | 3.00mm V-0,5VA |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 82.2 °C |
| | ASTMD648 | 76.1 °C |
| | ASTMD648 | 78.9 °C |
| | ASTMD648 | 72.2 °C |
| | ASTMD696 | 9E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.