Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|---|---|---|
Thermosetting mixed viscosity | ASTMD2393 | 375到850 cP | |
stripping time | 10到1400 min |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
ASTMD2240 | 59到94 |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile stress | ASTMD412 | 4.77到18.1 MPa | |
ASTMD412 | 7.71到31.4 MPa | ||
elongation | ASTMD412 | 300到600 % | |
tear strength | ASTMD624 | 49.0到132 kN/m | |
Split | ASTMD470 | 26 kN/m | |
compression set | ASTMD395 | 4.3到27 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.