Rubber Shin-Etsu Elastomer SV-14000U Shin-Etsu Silicones of America
Product Description
Certificates(0)
Datasheet
Product Description
Certificates
No Data...
Technical Data Sheet
| Uncured Properties | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Curing time | 0.17 | hr | ||
| elastomer | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | 100%Strain | 1.06 | MPa | |
| 5.12 | MPa | |||
| elongation | Break | 360 | % | |
| tear strength | 10.7 | kN/m | ||
| Permanent compression deformation | 177°C,22hr | 25 | % | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | 1.09 | g/cm³ | ||
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | 40 | |||
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| CureAgent | DCBP |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.