thermosettingTest ConditionTest MethodTest Result
STORAGE STABILITY5.0-6.0 min
Thermosetting mixed viscosityASTM D2393700 cP
stripping time2.0 min
Post curing time6.0 hr
physical property Test ConditionTest MethodTest Result
densityASTM D7921.08 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardnessShore AASTM D224091
elastomerTest ConditionTest MethodTest Result
tensile strength ASTM D4128.27 MPa
tensile strength ASTM D41213.8 MPa
tensile strength YieldASTM D41224.1 MPa
elongationBreakASTM D412300 %
compression setASTM D39526 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.