AS(SAN) KIBISAN®  PN-106L150

804
  • Properties:
    Chemical resistance
  • Usages:
    Automotive Interior Parts
    Toy
    Architectural Applications
    Industrial applications
    Monitor
  • Certificates:
    MSDS

Technical Data Sheet

otherTest ConditionTest MethodTest Result
notes加工指南:资料仅供参考.实际加工条件将依射出机之型式.模具之构造及成型性而调整。预热干燥2-3hrs:80-85℃;模温:40-60℃;射出缸温:180-230℃;射出压力:50-70kg/cm2。
Color透明
purpose蓄电池外壳.打火机外壳及要求较高强度之透明物体。
Mechanical propertiesTest ConditionTest MethodTest Result
elongationASTM D638/ISO 527800(11350) %
Rockwell hardnessASTM D78585
Flexural modulusASTM D790/ISO 1783.9(5.5) kg/cm²(MPa)[Lb/in²]
Physical propertiesTest ConditionTest MethodTest Result
densityASTM D792/ISO 11831.06 kg·cm/cm(J/M)ft·lb/in
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D648/ISO 7590 ℃(℉)
Heat distortion temperatureASTM D648/ISO 7588 ℃(℉)
melting temperature95 ℃(℉)
vicatASTM D1525/ISO R306128 ℃(℉)
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.