Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTMD792 | 1.22 g/cm³ | |
melt mass-flow rate | ASTMD1238 | 5.0到7.0 g/10min | |
relative viscosity | ASTMD5225 | 4.00 |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of cantilever beam gap | ASTMD256 | 320 J/m |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ASTMD638 | 2400 MPa | |
tensile strength | Yield | ASTMD638 | 32.8 MPa |
ASTMD638 | 30.0 MPa | ||
elongation | Break | ASTMD638 | 2.3 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | ASTME2092 | 80.0到90.0 °C | |
Glass Transition Temperature | ASTMD3418 | 55.0到60.0 °C | |
Crystallization peak temperature | ASTMD3418 | 165到180 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.