Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate | Saturation | ASTMD570 | 5.5 % |
density | | ASTMD792 | 1.16 g/cm³ |
Water absorption rate | | ASTMD570 | 0.55 % |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | R-Scale | ASTMD785 | 120 |
Shore Hardness | | ASTMD2240 | 81 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Compressive Modulus | | ASTMD695 | 2500 MPa |
compressive strength | | ASTMD695 | 102 MPa |
shear strength | | ASTMD732 | 72.4 MPa |
Coefficient of Friction | | ASTMD1894 | 0.22 |
Load deformation | | ASTMD621 | 1.50 % |
Tensile modulus | | ASTMD638 | 3280 MPa |
tensile strength | | ASTMD638 | 81.0 MPa |
elongation | Break | ASTMD638 | 38 % |
Flexural modulus | | ASTMD790 | 3170 MPa |
bending strength | | ASTMD790 | 114 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 43 J/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|
dielectric strength | | ASTMD149 | 22 kV/mm |
dielectric constant | | ASTMD150 | 3.70 |
dielectric constant | | ASTMD150 | 3.70 |
dielectric constant | | ASTMD150 | 3.70 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Heat Deflection Temperature | | ASTMD648 | 213 °C |
Heat Deflection Temperature | | ASTMD648 | 149 °C |
Continuous use temperature | | ASTMD794 | 110 °C |
melting temperature | | | 227到238 °C |
Linear thermal expansion coefficient | | ASTMD696 | 9E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.