PP LOXIM 820 01 HBCC LOXIM Industries Private Limited

0
  • Properties:
    Filler
    glass fiber reinforced material
    20%
    filler by weight

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7920.998to1.10 g/cm³
Shrinkage rateASTM D12990.60to0.80 %
densityASTM D7920.998to1.10 g/cm³
Shrinkage rateASTM D12990.60to0.80 %
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94HB
UL flame retardant ratingUL 94HB
Mechanical propertiesTest ConditionTest MethodTest Result
Flexural modulusASTM D7904000to4500 MPa
tensile strength BreakASTM D63870.0to80.0 MPa
elongationBreakASTM D6384.0to6.0 %
Flexural modulusASTM D7904000to4500 MPa
tensile strength BreakASTM D63870.0to80.0 MPa
elongationBreakASTM D6384.0to6.0 %
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTM D25680to100 J/m
Impact strength of cantilever beam gapASTM D25680to100 J/m
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D648B135to145 °C
Heat distortion temperatureASTM D648B135to145 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.