Polyester, TP MN631

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.19 g/cm³
Shrinkage rateASTMD9550.30 %
Water absorption rateASTMD5700.15 %
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessASTMD785107
optical performance Test ConditionTest MethodTest Result
transmissivityASTMD100392.0 %
Haze ratioASTMD1003<1.0 %
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthASTMD63850.0 MPa
tensile strengthASTMD63843.0 MPa
elongationASTMD6385.0 %
elongationASTMD638270 %
Flexural modulusASTMD7901900 MPa
bending strengthASTMD79068.0 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD25680 J/m
Impact strength of cantilever beam gapASTMD4812NoBreak
Impact strength of cantilever beam gapASTMD4812NoBreak
Dart impact equipped with measuring instrumentsASTMD376338.0 J
Dart impact equipped with measuring instrumentsASTMD376340.0 J
Impact strength of cantilever beam gapASTMD25644 J/m
Thermal performanceTest ConditionTest MethodTest Result
ASTMD64873.0 °C
ASTMD64866.0 °C
vicatASTMD1525286.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.