PA66 LUBEMID A26 GK50 NATURAL

0
  • Properties:
    Filler
    glass beads
    50%
    filler by weight

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO 11831.53to1.57 g/cm³
Mechanical propertiesTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapISO 180/1A3.50-4.50 kJ/m²
Suspended wall beam without notch impact strengthISO 180/1U35-45 kJ/m²
tensile strength ISO 527-255-65 MPa
elongation at breakISO 527-24.00-5.00 %
Tensile modulusISO 527-24000-4500 MPa
bending strengthISO 178105-115 MPa
Flexural modulusISO 1783000-4000 MPa
Charpy Notched Impact StrengthISO 179/1eA3.50-4.50 kJ/m²
Impact strength of simply supported beam without notchISO 179/1eU35-45 kJ/m²
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureISO 75-2/Bf230-240 °C
vicatMelting TemperatureISO 11357-3250-265 °C
Linear coefficient of thermal expansionISO 306/A120240-250 °C
Linear coefficient of thermal expansionISO 306/B120230-240 °C
Linear coefficient of thermal expansionASTM D648235-245 °C
Linear coefficient of thermal expansionASTM D64870-80 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.