PA66 9A22740 HFR5 4Plas
Properties:
Filler reinforcement material carbon fiber reinforcement material 40% filler additive by weight heat stabilizer characteristics thermal stability halogen-free
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | Filler | reinforcement material | carbon fiber reinforcement material | 40% | filler additive by weight | heat stabilizer characteristics | thermal stability | halogen-free |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 12 | kJ/m² |
| -30°C | ISO 180/1A | 11 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.60 mm | UL 94 | V-0 | |
| Burning wire flammability index | 1.0mm | IEC 60695-2-12 | 960 | °C |
| UL flame retardant rating | 1.6mm | UL 94 | V-0 | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | 23°C | ISO 527-2/5 | 40000 | MPa |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 12 | kJ/m² |
| -30°C | ISO 180/1A | 11 | kJ/m² | |
| Tensile strain | Break,23°C | ISO 527-2/5 | 1.0 | % |
| tensile strength | Break,23°C | ISO 527-2/5 | 220 | MPa |
| Tensile modulus | 23°C | ISO 527-2/5 | 40000 | MPa |
| Tensile strain | Break,23°C | ISO 527-2/5 | 1.0 | % |
| tensile strength | Break, 23°C | ISO 527-2/5 | 220 | MPa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Melting temperature | ISO 11357 | 262 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 245 | °C |
| 0.45MPa,Unannealed | ISO 75-2/B | 255 | °C | |
| Melting temperature | ISO 11357 | 262 | °C | |
| Hot deformation temperature | 1.8 MPa, Unannealed | ISO 75-2/A | 245 | °C |
| 0.45 MPa, Unannealed | ISO 75-2/B | 255 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 2.2 | % |
| water content | ISO 960 | <2000 | ppm | |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 2.2 | % |
| density | ISO 1183 | 1.52 | g/cm³ | |
| ISO 1183 | 1.52 | g/cm³ | ||
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Volume resistivity | IEC 60093 | 10 | ohms·cm | |
| Surface resistivity | IEC 60093 | <10 | ohms | |
| Volume resistivity | IEC 60093 | <10 | ohms·cm | |
| Surface resistivity | IEC 60093 | 10 | ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.