Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
melt mass-flow rate | ISO 1133 | 4.0 g/10min |
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Haze ratio | ASTM D1003 | 6.0 % | |
gloss | ASTM D2457 | 110 |
film | Test Condition | Test Method | Test Result |
---|---|---|---|
film thickness | 40 µm | ||
Secant modulus | ASTM D882A | 200 Mpa | |
ASTM D882A | 180 Mpa | ||
tensile strength | ISO 527-3 | 24.0 Mpa | |
ISO 527-3 | 18.0 Mpa | ||
elongation | ISO 527-3 | 400 % | |
ISO 527-3 | 650 % | ||
Dart impact | ISO 7765-1 | 80 g | |
Elmendorf tear strength | ISO 6383-2 | 3.0 N | |
ISO 6383-2 | 2.0 N |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
melting temperature | ISO 11357-3 | 111 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.