Rubber RTV-2 P-100 Silicones, Inc.
0
Technical Data Sheet
| Cured Properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Dissipation factor | 100Hz | 9E-03 | |
| Coverage-Cured | 0.802 cm³/g | ||
| Shore hardness | ShoreA5 | 26to34 | |
| ShoreA6 | 26to40 | ||
| tensile strength | ASTM D412 | 3.03to3.45 MPa | |
| elongation | Break | ASTM D412 | 320to370 % |
| tear strength | ASTM D624 | 10.5to14.0 kN/m | |
| Dielectric strength | 22 kV/mm | ||
| Relative permittivity | 100Hz | 2.10 | |
| Volume resistivity | 4.5E+14 ohms·cm |
| Uncured Properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Color | --3 | Brown | |
| --4 | OffWhite | ||
| viscosity | --4 | 30to50 Pa·s | |
| --3 | 1500to2500 Pa·s | ||
| 固化时间 | 16to24 hr | ||
| Pot Life | 60to120 min |
| thermosetting | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Thermosetting components | Resin | 按容量计算的混合比:100按重量计算的混合比:10 | |
| Hardener | 按容量计算的混合比:13按重量计算的混合比:1.0 | ||
| Shelf Life | 26 wk | ||
| 热固性混合粘度2 | 25000to40000 cP |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Usage temperature | 固化后 | -51-329 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | 1.25 g/cm³ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.