Rubber Silopren® LSR 2670 Momentive Performance Materials Inc.

0

Technical Data Sheet

thermosettingTest ConditionTest MethodTest Result
Thermosetting components按重量计算的混合比:1.0
Thermosetting components按重量计算的混合比:1.0
Thermosetting components4.0 hr
Uncured PropertiesTest ConditionTest MethodTest Result
ViscosityDIN 53018550 Pa·s
ViscosityDIN 53018550 Pa·s
ViscosityDIN 530184300 min
ColorTranslucent
ColorTranslucent
physical property Test ConditionTest MethodTest Result
densityDIN 534791.13 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardnessShore ADIN 5350569
Supplementary InformationTest ConditionTest MethodTest Result
sulfurization10.0 min
elastomerTest ConditionTest MethodTest Result
tear strengthASTM D62430.0 kN/m
compression setISO 81520 %
tensile strength DIN 535049.50 MPa
elongationBreakDIN 53504350 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.