PA66 KOPLA PA66 KDT1020

0
  • Properties:
    Filler
    KOPLA
    Korean Kopula
  • Usages:
    Bushing
    casing

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.28 g/cm³
Water absorption rateASTMD5700.50 %
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessR-ScaleASTMD785120
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL94HB
Mechanical propertiesTest ConditionTest MethodTest Result
elongationASTMD6385.0 %
Flexural modulusASTMD7904120 MPa
bending strengthASTMD790118 MPa
tensile strengthASTMD63873.5 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD25649 J/m
Electrical performanceTest ConditionTest MethodTest Result
Volume resistivityASTMD2571E+15 ohms·cm
dielectric strengthASTMD14920 kV/mm
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTMD648240 °C
Heat distortion temperatureASTMD648225 °C
Heat distortion temperatureMelting TemperatureASTMD648260 °C
ASTMD6966.5E-05 cm/cm/°C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.