Technical Data Sheet
processability | Test Condition | Test Method | Test Result |
---|
process temperature | | | 175-195 °C |
other | Test Condition | Test Method | Test Result |
---|
notes | | | 吹塑 其它 通用 |
characteristic | | | 流动性良、粘度稳定性优 |
purpose | | | 压延或吹塑成型 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ASTM D412 | >16.0 Mpa |
tear strength | | ASTM D624 | >110 N/mm |
Shore hardness | | ASTM D2240 | 95±2 |
Shore hardness | | ASTM D2240 | 无 |
compression set | | ASTM D395 | 40 % |
compression set | | ASTM D395 | 30 % |
Tensile modulus | | ASTM D412 | >8.0 Mpa |
wear resistance | | ASTM D1044 | 60 mg |
elongation | | ASTM D412 | >400 % |
Resilience | | ASTM D1054 | 35 % |
Tensile modulus | | ASTM D412/ISO 527 | >8.0 Mpa/Psi |
Tensile modulus | | ASTM D412/ISO 527 | >16.0 Mpa/Psi |
tensile strength | | ASTM D412/ISO 527 | >35.0 Mpa/Psi |
Shore hardness | | ASTM D2240/ISO 868 | 95±2 Shore A |
Other performance | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTM D412 | >35.0 Mpa |
Physical properties | Test Condition | Test Method | Test Result |
---|
density | | ASTM D792/ISO 2781/JIS K7311 | 1.20 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Low temperature softening temperature | | ASTM D1053 | -36 °C |
Glass transition temperature Tg | | ASTM D3417 | <-70 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.