PE ULV (3.50 pcf)

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D35750.0561 g/cm³
VOCContent5.5 %
VOCContent0.30 %
VOCContent0.900to2.00 mm
Supplementary InformationTest ConditionTest MethodTest Result
Puncture StrengthASTM D3763530 N
tear strengthASTM D35754.6 kN/m
Mechanical propertiesTest ConditionTest MethodTest Result
Bending StrainASTMC2037.7 %
bending strengthASTMC2030.797 MPa
bending strengthASTMC2030.834 MPa
compressive strengthASTM D35750.391 MPa
compressive strengthASTM D35750.450 MPa
compressive strengthASTM D35750.539 MPa
compressive strengthASTM D35751.11 MPa
tensile strength BreakASTM D35750.703 MPa
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.